10SG | pdb_000010sg

The CryoEM structure of T12 type1 nanofiber


ELECTRON MICROSCOPY
Sample
T12 type1 nanofiber
Specimen Preparation
Sample Aggregation StateFILAMENT
Vitrification Instrument
Cryogen NameETHANE
Sample Vitrification Details
3D Reconstruction
Reconstruction MethodHELICAL
Number of Particles35
Reported Resolution (Å)2.84
Resolution MethodFSC 0.143 CUT-OFF
Other Details
Refinement Type
Symmetry TypeHELICAL
Axial SymmetryC1
Axial Rise4.77
Angular Rotation-0.695
Map-Model Fitting and Refinement
Id1
Refinement Space
Refinement Protocol
Refinement Target
Overall B Value
Fitting Procedure
Details
Data Acquisition
Detector TypeFEI FALCON I (4k x 4k)
Electron Dose (electrons/Å**2)50
Imaging Experiment1
Date of Experiment
Temperature (Kelvin)
Microscope ModelTFS TALOS
Minimum Defocus (nm)1200
Maximum Defocus (nm)1800
Minimum Tilt Angle (degrees)
Maximum Tilt Angle (degrees)
Nominal CS
Imaging ModeBRIGHT FIELD
Specimen Holder Model
Nominal Magnification
Calibrated Magnification
SourceFIELD EMISSION GUN
Acceleration Voltage (kV)300
Imaging Details
EM Software
TaskSoftware PackageVersion
PARTICLE SELECTIONRELION
RECONSTRUCTIONServalcat
Image Processing
CTF Correction TypeCTF Correction DetailsNumber of Particles SelectedParticle Selection Details
PHASE FLIPPING ONLY